- If the focal point of the len shifts around the surface of the sample , the mass ablation , the temperature of the plasma and the spectral intensity appear asymmetric and their maximum occur at the location which is about 0 . 4mm under the surface of the sample . ( 2 ) to the plasma of the aluminum alloy sample , when the operating voltage is 1600v , the height from the observed location of the plasma to the surface of the sample is 2mm and the argon pressure is 660 torr , the spectral intensity have the maximum values
( 2 )对于标准铝样品,在激光器工作电压为1600v 、等离子体观测高度为2mm 、氩气压力为660乇时,其谱线强度最强;以al 308 . 22nm 、 al 309 . 27nm两条谱线为分析线,发现随着环境气压的增大,谱线自吸效应明显增强,当环境气压达到600 - 700乇时,谱线几乎产生自蚀。